Pavement design

Pavements are classified as:

Flexible pavement

In the flexible pavement, load from the top is distributed to the bottom layers through grain-to-grain contact.

We need to use better quality material in the top layers as compared to the bottom layers, because the stresses in the bottom layers would be lesser. Pavement layer thickness is decided in such a way that stresses in any layer do not exceed its permissible value.

In flexible pavement, any deformation in lower layers is reflected in top layers also.

Surface Base Sub-base Subgrade Subgrade = compacted soil

Flexible pavement layered cross-section: surface (thinnest, highest quality), base, sub-base, subgrade (compacted natural soil).

Purpose of various layers

1. Soil subgrade
The prepared soil which receives stresses from the upper layers.
2. Sub-base layer
A layer underneath the base layer; its priming function is to provide structural support, improve drainage, and reduce intrusion of fines into the pavement layers.
3. Base layer
Provided immediately below the wearing course (surface layer). It provides load distribution and contributes to sub-surface drainage. Generally composed of crushed stones.
4. Surface layer
The highest quality material. Provides smoothness, friction, drainage, and is generally made of bituminous mixes. Surface course resists heavy wheel loads, abrasive action of the wheels, and weathering effects.

Failure of flexible pavement

Major flexible pavement failures are:

IRC code considers fatigue cracking and rutting for flexible pavement design.

Fatigue cracks — 20% of total area

In fatigue cracks, tensile strength at the bottom of the pavement surface layer is considered. An area of 20% of total surface area having fatigue cracks is considered critical.

Crocodile cracking

Crocodile (fatigue) cracking pattern — interlinked cracks over the critical 20% area, governed by tensile strain at the bottom of the surface layer.

Rutting — 20 mm deflection

Compressive strain at the top of the subgrade layer is considered critical for rutting. Deflection of 20 mm at the top of the subgrade layer is considered critical.

Rigid pavements

Load resistance in rigid pavements is by flexural action of the slab.

PWP Subgrade Surface Base

Rigid pavement slab on base and subgrade; PWP = pumping water pressure at the joint under wheel load.

The purpose of the base layer in this case is to prevent pumping and provide drainage.

Failure of rigid pavements

NoteIRC code gives design steps only for fatigue cracking.

Allowable number of load repetitions depends on the stress ratio.

Stress ratio Stress ratio=flexural stressmodulus of rupture of concrete

For stress ratio less than 0.5, the allowable number of load repetitions tends to infinity.